Canada Spends Logo

Explore our Budget 2026 analysis

Grant: Collaborative Research and Development Grants

University of British Columbia

$24,000.00

High Pressure and Temperature Cobalt Cementation

FY 2013-14

Summary
Before zinc electrowinning, cobalt must be removed from the electrolyte to concentrations typically less than 0.3 mg/L. Cobalt is highly detrimental to the electrowinning process as it catalyzes hydrogen evolution and diverts almost the entire cell current to hydrogen production rather than zinc electro-reduction. The standard practice for the removal of cobalt from zinc sulphate electrolytes is cementation onto zinc dust. This process is inefficient. It requires that large reactors be heated to temperatures near the boiling point for 2-3 hours. In addition, zinc utilization is high in this cementation process. Activators are also required to enhance the rate of cementation such that retention times do not exceed 3 hours. One such system of activation is the inclusion of antimony (1.5 mg L-1) and copper (30 mg L-1) with the zinc dust. We propose to study the high pressure and temperature cementation of cobalt in order to increase the rate and efficiency of this process. The increased temperature and pressure is expected to substantially increase the rate of reaction: from 2-3 hours under currently practiced conditions to less than 40 minutes under the proposed conditions. The study proposed herein is fundamental and will report the kinetics and morphological development during cobalt cementation onto zinc dust under novel conditions. In addition to conventional measurement of reaction kinetics, the cobalt cements will be analyzed by scanning electron microscopy, electron microprobe and X-Ray diffraction to elucidate the mechanism(s) of cementation as a function of pressure and temperature.
Program
Collaborative Research and Development Grants
Location
British Columbia, Canada
Recipient Type
Academia
Type
Grant
Source
NSERC's Awards Data

As published

Application id
428472-2011
Name nom
Asselin, Edouard
Department département
Materials Engineering
Organization id
2
Institution établissement
University of British Columbia
Province en
British Columbia
Province fr
Colombie-Britannique
Country en
CANADA
Country fr
CANADA
Fiscal year exercice financier
2013
Competition year année de concours
2011
Award amount
24000
Program id
CRDPJ
Program name en
Collaborative Research and Development Grants
Program name fr
Subventions de recherche et développement coopérative
Group en
Research partnerships programs
Group fr
Programmes de partenariat
Committee code
96
Committee name en
RPP Internal Decision Cttee
Committee name fr
Cté de décision interne - PPR
Area of application code
202
Area of application group en
Natural resources (economic aspects)
Area of application group fr
Ressources naturelles (aspects économiques)
Area of application en
Mineral resources ( prospecting, exploration, mining, extraction, processing)
Area of application fr
Ressources minérales (prospection, exploration, mines, extraction et préparation)
Research subject code
2003
Research subject group en
Materials science and technology
Research subject group fr
Science et technologie des matériaux
Research subject en
Metallurgy
Research subject fr
Métallurgie
Partie
2
Nb partie
2
Application title
High Pressure and Temperature Cobalt Cementation
Keyword
NSERC
Application summary
Before zinc electrowinning, cobalt must be removed from the electrolyte to concentrations typically less than 0.3 mg/L. Cobalt is highly detrimental to the electrowinning process as it catalyzes hydrogen evolution and diverts almost the entire cell current to hydrogen production rather than zinc electro-reduction. The standard practice for the removal of cobalt from zinc sulphate electrolytes is cementation onto zinc dust. This process is inefficient. It requires that large reactors be heated to temperatures near the boiling point for 2-3 hours. In addition, zinc utilization is high in this cementation process. Activators are also required to enhance the rate of cementation such that retention times do not exceed 3 hours. One such system of activation is the inclusion of antimony (1.5 mg L-1) and copper (30 mg L-1) with the zinc dust. We propose to study the high pressure and temperature cementation of cobalt in order to increase the rate and efficiency of this process. The increased temperature and pressure is expected to substantially increase the rate of reaction: from 2-3 hours under currently practiced conditions to less than 40 minutes under the proposed conditions. The study proposed herein is fundamental and will report the kinetics and morphological development during cobalt cementation onto zinc dust under novel conditions. In addition to conventional measurement of reaction kinetics, the cobalt cements will be analyzed by scanning electron microscopy, electron microprobe and X-Ray diffraction to elucidate the mechanism(s) of cementation as a function of pressure and temperature.