Grant: Collaborative Research and Development Grants
University of Waterloo
$41,304.00
Synthesis and characterization of butyl rubber ionomers
FY 2010-11
Summary
Butyl rubber (isobutylene-isoprene rubber, IIR) is a material with unusual physical properties, useful in different areas including automotive, architectural, and biomedical applications. A good resilience (shape recovery upon deformation) is necessary for all these applications. This is possible for IIR because the polymer chains contain a low concentration (1-2%) of isoprene (unsaturated) units in addition to isobutylene, allowing covalent (permanent) cross-linking of the chains into a 3-dimensional network structure. The covalent bonding approach, while providing good dimensional stability, allows only limited control over the mechanical properties of the material. Ionic interactions, on the other hand, are known to be very useful to modify the mechanical properties (e.g. rigidity, softening temperature, tear resistance) of rubbers and plastics, and have found applications in commercial products such as the Surlyn? resins, used as highly tear-resistant materials for blister packaging. The improved properties of polymers containing a low concentration of polymer-bound ionic groups (ionomers) are attributed to the aggregation of the ionic moieties, acting as multivalent physical cross-links at low to moderate temperatures. The application of the ionomer concept to improve the mechanical properties of butyl rubber has received little attention, mainly due to the very low (1-2%) isoprene content achieved in the traditional butyl rubber synthesis. New processes developed recently at LANXESS Inc. allow the synthesis of butyl rubber containing 1) up to 5-6% of isoprene units, or 2) up to 10% of p-methylstyrene units. This would allow the synthesis of ionomers with higher ionic moieties contents, and correspondingly a much wider range of mechanical properties than for traditional IIR. In the proposed project, reaction conditions will be established for the derivatization of high isoprene content IIR and of p-methylstyrene-modified IIR to novel ionomers by different techniques, and the mechanical properties of the resulting polymers will be investigated to correlate their structure with the observed properties. These butyl rubber ionomers are emerging materials of interest for applications in areas including the automotive industry.
Program
Collaborative Research and Development Grants
Recipient
Location
Ontario, Canada
Recipient Type
Academia
Type
Grant
Source
NSERC's Awards Data
As published
Application id
372569-2008
Name nom
Gauthier, Mario
Department département
Chemistry
Organization id
33
Institution établissement
University of Waterloo
Province en
Ontario
Province fr
Ontario
Country en
CANADA
Country fr
CANADA
Fiscal year exercice financier
2010
Competition year année de concours
2008
Award amount
41304
Program id
CRDPJ
Program name en
Collaborative Research and Development Grants
Program name fr
Subventions de recherche et développement coopérative
Group en
Research partnerships programs
Group fr
Programmes de partenariat
Committee code
96
Committee name en
RPP Internal Decision Cttee
Committee name fr
Cté de décision interne - PPR
Area of application code
508
Area of application group en
Manufacturing processes and products
Area of application group fr
Procédés et produits industriels
Area of application en
Polymers, rubber and plastics
Area of application fr
Polymères, caoutchouc et plastiques
Research subject code
3751
Research subject group en
Polymer chemistry
Research subject group fr
Chimie des polymères
Research subject en
Polymer synthesis
Research subject fr
Synthèse des polymères
Partie
2
Nb partie
2
Application title
Synthesis and characterization of butyl rubber ionomers
Keyword
NSERC
Application summary
Butyl rubber (isobutylene-isoprene rubber, IIR) is a material with unusual physical properties, useful in different areas including automotive, architectural, and biomedical applications. A good resilience (shape recovery upon deformation) is necessary for all these applications. This is possible for IIR because the polymer chains contain a low concentration (1-2%) of isoprene (unsaturated) units in addition to isobutylene, allowing covalent (permanent) cross-linking of the chains into a 3-dimensional network structure. The covalent bonding approach, while providing good dimensional stability, allows only limited control over the mechanical properties of the material. Ionic interactions, on the other hand, are known to be very useful to modify the mechanical properties (e.g. rigidity, softening temperature, tear resistance) of rubbers and plastics, and have found applications in commercial products such as the Surlyn? resins, used as highly tear-resistant materials for blister packaging. The improved properties of polymers containing a low concentration of polymer-bound ionic groups (ionomers) are attributed to the aggregation of the ionic moieties, acting as multivalent physical cross-links at low to moderate temperatures. The application of the ionomer concept to improve the mechanical properties of butyl rubber has received little attention, mainly due to the very low (1-2%) isoprene content achieved in the traditional butyl rubber synthesis. New processes developed recently at LANXESS Inc. allow the synthesis of butyl rubber containing 1) up to 5-6% of isoprene units, or 2) up to 10% of p-methylstyrene units. This would allow the synthesis of ionomers with higher ionic moieties contents, and correspondingly a much wider range of mechanical properties than for traditional IIR. In the proposed project, reaction conditions will be established for the derivatization of high isoprene content IIR and of p-methylstyrene-modified IIR to novel ionomers by different techniques, and the mechanical properties of the resulting polymers will be investigated to correlate their structure with the observed properties. These butyl rubber ionomers are emerging materials of interest for applications in areas including the automotive industry.