Understanding the microstructural bonding mechanisms between Y-TZP and veneering ceramic
FY 2022-23
Summary
Dental veneered zirconia-based core restorations have been used widely to date. The zirconia core is layered with a porcelain veneer material to achieve suitable esthetics. However, zirconia-based restorations can create clinical issues such as chipping or fracture of the porcelain veneered layer. Previous studies have reported a significant incidence of veneer failures such as delaminations, chipping and cracking. This fracture behavior could be attributed to the poor veneer/core interface bond strength, elastic modulus mismatch between the core material and the veneer, coefficient of thermal expansion mismatch between the core and the veneer, weak porcelain strength and thermal procedure which could introduce residual stress induced by cooling rate and/or sintering at high temperatures. To improve the compatibility at the interface between veneer and core, and to avoid premature failure, the interface zirconia/porcelain should be better understood. The proposed research will investigate the detailed mechanism for the adhesion at the interface zirconia/porcelain to develop a feasible solution to improve the bonding between these two materials, using both molding techniques (the layering technique and the press technique). The thermal stresses will be also evaluated. The main objectives of this study are to characterize the interaction between porcelain and zirconia then, materials or new designs will be developed based on the results. Therefore, better bonding stability between porcelain veneer and zirconia core of an all-ceramic restoration can be achieved. The adhesion of porcelain veneer to zirconia is fundamental for the success of the zirconia-based restorations. After determining the new protocol and/or design to fabricate zirconia-based restorations, mechanical tests will be performed.Different tests will be carefully conducted to describe the microstructural mechanisms of zirconia/porcelain bond. The tests are SEM, EDS, Electron Backscatter Diffraction (EBSD). Furthermore, microstructures, texture, defects, grain morphology and deformation will also be evaluated by EBSD. In addition, the Focused Ion Beam microscopy (FIB) will be used to prepare thin specimens for the TEM and for Time-of-Flight Secondary Ion Mass Spectrometry (TOF-SIMS). Auger Microprobe will contribute to the determination of 2D and 3D elemental distributions on surfaces with high spatial resolution. The bond formation of the zirconia to porcelain will also be examined by XPS.The outcome of the research is to provide the dental laboratories with a new protocol to fabricate dental veneered zirconia-based core restorations in order to improve the success rate of this type of dental restoration. The new protocol will be based on the detailed bond mechanisms at the zirconia/porcelain interface obtained from the results of this study. Over 5 years, I will train 3 graduate students.
Program
Discovery Grants Program - Individual
Recipient
Location
Ontario, Canada
Recipient Type
Academia
Type
Grant
Source
NSERC's Awards Data
As published
Application id
RGPIN-2016-05178
Name nom
Butler, Sheila
Department département
Dentistry - Dentistry
Organization id
36
Institution établissement
University of Western Ontario
Province en
Ontario
Province fr
Ontario
Country en
CANADA
Country fr
CANADA
Fiscal year exercice financier
2022
Competition year année de concours
2016
Award amount
25000
Program id
RGPIN
Program name en
Discovery Grants Program - Individual
Program name fr
Programme de subventions à la découverte - individuelles
Group en
DISCOVERY RESEARCH
Group fr
RECHERCHE AXÉE SUR LA DÉCOUVERTE
Committee code
1511
Committee name en
Materials and Chemical Engineering
Committee name fr
Génie chimique et des matériaux
Area of application code
1211
Area of application group en
Advancement of knowledge
Area of application group fr
Avancement des connaissances
Area of application en
Medical and health sciences
Area of application fr
Sciences médicales et de la santé
Research subject code
9000
Research subject group en
Medical sciences
Research subject group fr
Sciences médicales
Research subject en
Medical sciences
Research subject fr
Sciences médicales
Installment
inst:7
Partie
1
Nb partie
8
Application title
Understanding the microstructural bonding mechanisms between Y-TZP and veneering ceramic
Application summary
Dental veneered zirconia-based core restorations have been used widely to date. The zirconia core is layered with a porcelain veneer material to achieve suitable esthetics. However, zirconia-based restorations can create clinical issues such as chipping or fracture of the porcelain veneered layer. Previous studies have reported a significant incidence of veneer failures such as delaminations, chipping and cracking. This fracture behavior could be attributed to the poor veneer/core interface bond strength, elastic modulus mismatch between the core material and the veneer, coefficient of thermal expansion mismatch between the core and the veneer, weak porcelain strength and thermal procedure which could introduce residual stress induced by cooling rate and/or sintering at high temperatures. To improve the compatibility at the interface between veneer and core, and to avoid premature failure, the interface zirconia/porcelain should be better understood. The proposed research will investigate the detailed mechanism for the adhesion at the interface zirconia/porcelain to develop a feasible solution to improve the bonding between these two materials, using both molding techniques (the layering technique and the press technique). The thermal stresses will be also evaluated. The main objectives of this study are to characterize the interaction between porcelain and zirconia then, materials or new designs will be developed based on the results. Therefore, better bonding stability between porcelain veneer and zirconia core of an all-ceramic restoration can be achieved. The adhesion of porcelain veneer to zirconia is fundamental for the success of the zirconia-based restorations. After determining the new protocol and/or design to fabricate zirconia-based restorations, mechanical tests will be performed.Different tests will be carefully conducted to describe the microstructural mechanisms of zirconia/porcelain bond. The tests are SEM, EDS, Electron Backscatter Diffraction (EBSD). Furthermore, microstructures, texture, defects, grain morphology and deformation will also be evaluated by EBSD. In addition, the Focused Ion Beam microscopy (FIB) will be used to prepare thin specimens for the TEM and for Time-of-Flight Secondary Ion Mass Spectrometry (TOF-SIMS). Auger Microprobe will contribute to the determination of 2D and 3D elemental distributions on surfaces with high spatial resolution. The bond formation of the zirconia to porcelain will also be examined by XPS.The outcome of the research is to provide the dental laboratories with a new protocol to fabricate dental veneered zirconia-based core restorations in order to improve the success rate of this type of dental restoration. The new protocol will be based on the detailed bond mechanisms at the zirconia/porcelain interface obtained from the results of this study. Over 5 years, I will train 3 graduate students.