Residual stress-based post-weld treatments, such as needle peening or ultrasonic impact treatment (UIT), are one way of improving the fatigue performance of new and existing welded structures. Typically these treatments involve impacting the weld "toe" in such a way as to cause plastic deformations, resulting in the formation of a thin compressive residual stress layer near the treated surface. This layer increases fatigue life by reducing crack propagation rates at smaller crack depths.
To date, only a small number of studies have examined the application of post-weld treatments under load. The results of these studies have suggested that these treatments should be even more effective, in particular for civil engineering applications, if they are applied after the permanent self weight or "dead load" stresses are introduced. No attempt has been made to date, however, to measure the stress distributions in welds that have been treated under load. What's more, no design (S-N) curves exist that consider the greater fatigue life increase that may result from treatment after the dead load stresses have been introduced. Whether the treatment is intended to improve the performance of new civil structures or to extend the service life of existing ones, some way of reliably predicting this additional fatigue life increase should result in significant economic benefits for owners of civil infrastructure in Canada and abroad.
Based on the above discussion, the main objective of the project described herein will be to conduct the research- and synthesis-related work required to develop a set of design curves for welds that have been treated by peening or ultrasonic impact treatment under load. The proposed methodology will comprise a combination of laboratory fatigue tests on welded steel specimens, residual stress measurements, and analytical studies performed using a strain-based fracture mechanics approach. The work will be undertaken as part of a graduate level thesis project. Additional support for this research will be provided by the Canadian Institute of Steel Construction (CISC) - Steel Structures Education Foundation (SSEF).
Program
Collaborative Research and Development Grants
Recipient
Location
Ontario, Canada
Recipient Type
Academia
Type
Grant
Source
NSERC's Awards Data
As published
Application id
380034-2008
Name nom
Walbridge, Scott
Department département
Civil & Environmental Engineering
Organization id
33
Institution établissement
University of Waterloo
Province en
Ontario
Province fr
Ontario
Country en
CANADA
Country fr
CANADA
Fiscal year exercice financier
2009
Competition year année de concours
2008
Award amount
9039
Program id
CRDPJ
Program nane en
Collaborative Research and Development Grants
Program name fr
Subventions de recherche et développement coopérative
Group en
Research partnerships programs
Group fr
Programmes de partenariat
Committee code
96
Committee name en
RPP Internal Decision Cttee
Committee name fr
Cté de décision interne - PPR
Area of application code
601
Area of application group en
Construction, urban and rural planning
Area of application group fr
Construction, urbanisme et aménagement rural
Area of application en
Structural engineering
Area of application fr
Génie des charpentes
Research subject code
1102
Research subject group en
Structural engineering
Research subject group fr
Génie des structures
Research subject en
Steel structures
Research subject fr
Structures en acier
Partie
1
Nb partie
2
Application title
Predicting the Effectiveness of Post-Weld Treatments Applied under Load
Keyword
NA
Application summary
Residual stress-based post-weld treatments, such as needle peening or ultrasonic impact treatment (UIT), are one way of improving the fatigue performance of new and existing welded structures. Typically these treatments involve impacting the weld "toe" in such a way as to cause plastic deformations, resulting in the formation of a thin compressive residual stress layer near the treated surface. This layer increases fatigue life by reducing crack propagation rates at smaller crack depths.
To date, only a small number of studies have examined the application of post-weld treatments under load. The results of these studies have suggested that these treatments should be even more effective, in particular for civil engineering applications, if they are applied after the permanent self weight or "dead load" stresses are introduced. No attempt has been made to date, however, to measure the stress distributions in welds that have been treated under load. What's more, no design (S-N) curves exist that consider the greater fatigue life increase that may result from treatment after the dead load stresses have been introduced. Whether the treatment is intended to improve the performance of new civil structures or to extend the service life of existing ones, some way of reliably predicting this additional fatigue life increase should result in significant economic benefits for owners of civil infrastructure in Canada and abroad.
Based on the above discussion, the main objective of the project described herein will be to conduct the research- and synthesis-related work required to develop a set of design curves for welds that have been treated by peening or ultrasonic impact treatment under load. The proposed methodology will comprise a combination of laboratory fatigue tests on welded steel specimens, residual stress measurements, and analytical studies performed using a strain-based fracture mechanics approach. The work will be undertaken as part of a graduate level thesis project. Additional support for this research will be provided by the Canadian Institute of Steel Construction (CISC) - Steel Structures Education Foundation (SSEF).