Delayed Hydride Cracking in Zirconium during Heat up and at Low Temperatures

EF 2010-11

Résumé
DHC is a thermally activated 'slow-cracking' mechanism, occurring in Zr-2.5Nb CANDU pressure tubes when hydrogen (deuterium) is found above a critical concentration, diffuses to stress concentrations at a crack tip (or other stress concentrater) and precipitates as hydrides. When these brittle hydrides are large enough, they crack, the crack propagates and arrests at the ductile matrix and the process repeats. Above temperatures of around 200°C the DHC mechanism is reasonably well understood, with observed hydride characteristics and crack velocity in good agreement with model predictions. However, at temperatures below 200°C there is a transition in the DHC behaviour, which is not well understood. Specifically, below ~200°C cracks can be initiated without thermal cycling, and even during heat up; while in the regime above 200°C, it is known that cracks initiate only after cool down. Further, the crack velocity at these lower temperatures is observed to be somewhat higher than would be expected based on extrapolation of data from above 200°C. This may be associated with a phase change in the hydrides (observed at 150-180°C). The project addresses the low temperature (i.e. <200°C) formation of hydrides, and in particular the occurrence of DHC during heat up. We will carry out a series of experiments on typical pressure tube microstructure material, for different hydrogen concentrations, stresses, heating rates, dwell temperatures and times.
Programme
Collaborative Research and Development Grants
Bénéficiaire
Emplacement
Ontario, Canada
Type de bénéficiaire
Academia
Type
Grant
Source
NSERC's Awards Data

Tel que publié

Application id
370874-2008
Name nom
Daymond, Mark
Department département
Mechanical and Materials Engineering
Organization id
29
Institution établissement
Queen's University
Province en
Ontario
Province fr
Ontario
Country en
CANADA
Country fr
CANADA
Fiscal year exercice financier
2010
Competition year année de concours
2008
Award amount
37500
Program id
CRDPJ
Program name en
Collaborative Research and Development Grants
Program name fr
Subventions de recherche et développement coopérative
Group en
Research partnerships programs
Group fr
Programmes de partenariat
Committee code
96
Committee name en
RPP Internal Decision Cttee
Committee name fr
Cté de décision interne - PPR
Area of application code
1208
Area of application group en
Advancement of knowledge
Area of application group fr
Avancement des connaissances
Area of application en
Materials sciences
Area of application fr
Sciences des matériaux
Research subject code
2001
Research subject group en
Materials science and technology
Research subject group fr
Science et technologie des matériaux
Research subject en
Materials structure, properties and testing
Research subject fr
Structure, propriétés et essais des matériaux
Partie
3
Nb partie
3
Application title
Delayed Hydride Cracking in Zirconium during Heat up and at Low Temperatures
Keyword
NSERC
Application summary
DHC is a thermally activated 'slow-cracking' mechanism, occurring in Zr-2.5Nb CANDU pressure tubes when hydrogen (deuterium) is found above a critical concentration, diffuses to stress concentrations at a crack tip (or other stress concentrater) and precipitates as hydrides. When these brittle hydrides are large enough, they crack, the crack propagates and arrests at the ductile matrix and the process repeats. Above temperatures of around 200°C the DHC mechanism is reasonably well understood, with observed hydride characteristics and crack velocity in good agreement with model predictions. However, at temperatures below 200°C there is a transition in the DHC behaviour, which is not well understood. Specifically, below ~200°C cracks can be initiated without thermal cycling, and even during heat up; while in the regime above 200°C, it is known that cracks initiate only after cool down. Further, the crack velocity at these lower temperatures is observed to be somewhat higher than would be expected based on extrapolation of data from above 200°C. This may be associated with a phase change in the hydrides (observed at 150-180°C). The project addresses the low temperature (i.e. <200°C) formation of hydrides, and in particular the occurrence of DHC during heat up. We will carry out a series of experiments on typical pressure tube microstructure material, for different hydrogen concentrations, stresses, heating rates, dwell temperatures and times.